ZG15Cr2Mo1合金鑄件吊耳斷裂原因分析ZG15Cr2Mo1合金鑄件吊耳斷裂原因分析Cause Analysis on Fracture of ZG15Cr2Mo1 Alloy Casting's Lifting Handle 某ZG15Cr2Mo1合金鑄件吊耳在吊運過程中發生斷裂,通過宏觀觀察、化學成分分析、力學性能測試、金相檢驗、高溫拉伸試驗、蠕變試驗等方法對吊耳斷裂原因進行了分析。結果表明:該鑄件吊耳本身晶粒粗大,沖擊吸收能量低,且過渡圓角小,應力在該處集中,加之在鑄件吊運過程中操作不當,使得吊耳受到撞擊而斷裂。 The ZG15Cr2Mo1 alloy casting's lifting handle fractured during the lifting process. The fracture reasons of the lifting handle were analyzed by means of macro observation, chemical composition analysis, mechanical property test, metallographic test, high temperature tensile test, creep test and so on. The results show that the casting's lifting handle grains was coarse, and its impact absorption energy was low and the transition fillet was small, and the stress was concentrated in the area. Improper operation during the lifting process of the casting caused the lifting handle to fracture by impact. 全文下載:https://pan.baidu.com/s/18xYEANFvXUNzdaHtgp0L8g? 作為值得信賴的合作伙伴和高品質金屬合金的半成品供應商,通項公司擁有完善的服務體系和專業的團隊。在同客戶交易的過程中,我們力求根據不同的應用需求將我們的產品做到精益求精。針對當前和未來的市場需求,通項公司致力于為客戶提供優質的金屬材料解決方案。 TXCO has been a reliable partner and supplier of sophisticated and high-quality semi-finished products maed of alloys. In dialogue with our customers, we optimise our products to meet the specific application requirements. TXCO develops the superior alloy material solutions for current and future challenges. 獲取更多我們供應的產品和服務信息,請致電086-021-6786 0205或發電子郵件service@sinoav.com聯系我們,您也可以通過微信,微博,領英,臉書,推特和谷歌+與我們互動。 For more information on the products and services that we supply, call us at 086-021-6786 0205 or email us at service@sinoav.com. You can also get in touch on social media, we are constantly active on Weixin, Weibo, LinkedIn, Facebook, Twitter and Google+. 上一篇: 鐵素體不銹鋼晶粒度的非線性超聲表征
|