A335P11鋼在流動加速腐蝕條件下的管壁減薄行為A335P11鋼在流動加速腐蝕條件下的管壁減薄行為Pipeline Wall Thinning Behavior of A335P11 Steel under the Condition of Flow Accelerated Corrosion 模擬了核電廠常規島二回路工況,研究了此工況條件下A335P11鋼彎管測試段、變徑測試段及三通測試段的腐蝕減薄現象。結果表明:發生流動加速腐蝕(FAC)最嚴重的部位是彎管內弧面、變徑管的漸縮管段出口處以及三通測試段的輔出水口處。 The conditions of the second loop of the conventional island in nuclear power plant were simulated, and the corrosion thinning behavior of A335P11 pipeline in elbow test section, variable diameter test section and three-way test section under this working condition was studied. The results showed that the most serious site of FAC occured at the inner arc surface of the elbow, the outlet of tapered pipe section of the adjustable pipe, and the auxiliary outlet of the three-way test section. 全文下載:https://pan.baidu.com/s/1DzHktUwknqSsgdxOUWkZrw? 作為值得信賴的合作伙伴和高品質金屬合金的半成品供應商,通項公司擁有完善的服務體系和專業的團隊。在同客戶交易的過程中,我們力求根據不同的應用需求將我們的產品做到精益求精。針對當前和未來的市場需求,通項公司致力于為客戶提供優質的金屬材料解決方案。 TXCO has been a reliable partner and supplier of sophisticated and high-quality semi-finished products maed of alloys. In dialogue with our customers, we optimise our products to meet the specific application requirements. TXCO develops the superior alloy material solutions for current and future challenges. 獲取更多我們供應的產品和服務信息,請致電086-021-6786 0205或發電子郵件service@sinoav.com聯系我們,您也可以通過微信,微博,領英,臉書,推特和谷歌+與我們互動。 For more information on the products and services that we supply, call us at 086-021-6786 0205 or email us at service@sinoav.com. You can also get in touch on social media, we are constantly active on Weixin, Weibo, LinkedIn, Facebook, Twitter and Google+.
|