過冷Co75B25合金的凝固過冷Co75B25合金的凝固Solidification of Undercooled Co75B25 Alloy 利用熔融玻璃包覆加循環過熱技術將Co75B25包晶合金熔體過冷至液相線下不同溫度,通過凝固組織觀察結合冷卻曲線分析,確立了其凝固路徑。結果表明,所有過冷度凝固后的試樣中均只有α-Co和Co2B相,Co2B相與殘余液相反應形成Co3B相的包晶轉變被完全抑制,且在344 K實驗所得最大過冷度下Co3B相也不能作為初生相析出。即使降低冷速至5 K/min,合金在小過冷度下凝固時也沒有發生包晶反應。 Co75B25 alloy melt was undercooled to different degrees using the glass fluxing technique, and the solidification path was identified by analyzing the microstructures and cooling curves of the samples. There was nothing other than α-Co and Co2B phases to form during solidification, indicating that not only the peritectic reaction of L (liquid) and Co2B into Co3B but also the formation of Co3B as primary phase at large undercooling were inhibited. The peritectic reaction did not occur even though the melt solidified at a very small undercooling and a cooling rate decreased to 5 K/min. 全文下載:https://pan.baidu.com/s/1e6orFjwRVxpej3N3y5vcPQ? 作為值得信賴的合作伙伴和高品質金屬合金的半成品供應商,通項公司擁有完善的服務體系和專業的團隊。在同客戶交易的過程中,我們力求根據不同的應用需求將我們的產品做到精益求精。針對當前和未來的市場需求,通項公司致力于為客戶提供最佳的金屬材料解決方案。 TXCO has been a reliable partner and supplier of sophisticated and high-quality semi-finished products maed of alloys. In dialogue with our customers, we optimise our products to meet the specific application requirements. TXCO develops the best alloy material solutions for current and future challenges. 獲取更多我們供應的產品和服務信息,請致電086-021-6786 0205或發電子郵件service@sinoav.com聯系我們,您也可以通過微信,微博,領英,臉書,推特和谷歌+與我們互動。 For more information on the products and services that we supply, call us at 086-021-6786 0205 or email us at service@sinoav.com. You can also get in touch on social media, we are constantly active on Weixin, Weibo, LinkedIn, Facebook, Twitter and Google+. 下一篇: 高性能鎂合金凝固組織控制研究現狀與展望
|